Nickel-saving austenitic stainless steel, which uses manganese and nitrogen to replace nickel, contains about 16-18% chromium and about 3.5-5.5% nickel.
High-manganese, low-nickel austenitic stainless steel contains approximately 17-19% chromium and 4-6% nickel.
Metastable austenitic stainless steel contains approximately 16-18% chromium and 6-8% nickel.
Type 18-8 austenitic stainless steel contains approximately 18% chromium and 8% nickel.
Free-machining austenitic stainless steel, with added elements such as sulfur and selenium to improve its machinability, contains approximately 18% chromium and 9% nickel, making it suitable for high-speed automatic machine tool processing.
The most common type, 18-8 austenitic stainless steel, contains approximately 18-20% chromium and 8-10.5% nickel.
Ultra-low carbon 304 stainless steel, with a carbon content of ≤0.03%, has excellent resistance to intergranular corrosion.
High-nickel austenitic stainless steel has a nickel content of approximately 10-13%, low work hardening rate, and excellent cold forming performance, making it suitable for deep drawing and complex cold working.
High-chromium-nickel heat-resistant austenitic stainless steel contains approximately 22-24% chromium and 12-15% nickel.
Ultra-low carbon high chromium nickel heat-resistant austenitic stainless steel, containing about 25% chromium and about 20% nickel, has excellent high-temperature oxidation resistance and can be used continuously below 1200℃.
Molybdenum-containing austenitic stainless steel contains approximately 16-18% chromium, 10-14% nickel, and 2-3% molybdenum.
Ultra-low carbon molybdenum-containing austenitic stainless steel with a carbon content of ≤0.03% exhibits excellent resistance to intergranular corrosion, good weldability, and superior corrosion resistance compared to 316.