305 stainless steel bar

High-nickel austenitic stainless steel has a nickel content of approximately 10-13%, low work hardening rate, and excellent cold forming performance, making it suitable for deep drawing and complex cold working.

309/309S stainless steel bar

High-chromium-nickel heat-resistant austenitic stainless steel contains approximately 22-24% chromium and 12-15% nickel.

310S stainless steel bar

Ultra-low carbon high chromium nickel heat-resistant austenitic stainless steel, containing about 25% chromium and about 20% nickel, has excellent high-temperature oxidation resistance and can be used continuously below 1200℃.

316 stainless steel bar

Molybdenum-containing austenitic stainless steel contains approximately 16-18% chromium, 10-14% nickel, and 2-3% molybdenum.

316L stainless steel bar

Ultra-low carbon molybdenum-containing austenitic stainless steel with a carbon content of ≤0.03% exhibits excellent resistance to intergranular corrosion, good weldability, and superior corrosion resistance compared to 316.

316Ti stainless steel bar

Titanium-stabilized molybdenum-containing austenitic stainless steel has excellent resistance to intergranular corrosion, high high-temperature strength, and good weldability due to the addition of titanium to stabilize carbides.

317L stainless steel bar

High-molybdenum ultra-low carbon austenitic stainless steel, with a molybdenum content of 3-4%, has better resistance to pitting and crevice corrosion than 316L, making it suitable for more severe corrosive environments.

321 stainless steel bar

Titanium-stabilized austenitic stainless steel, with the addition of titanium to prevent intergranular corrosion, has high high-temperature strength, good oxidation resistance, and excellent weldability.

330 stainless steel bar

High-nickel-chromium heat-resistant alloys, with a nickel content of 34-37% and a chromium content of 17-20%, exhibit excellent resistance to high-temperature oxidation and carburization, as well as superior resistance to thermal fatigue.

347 stainless steel bar

Niobium-stabilized austenitic stainless steel, with the addition of niobium to stabilize carbides, exhibits excellent resistance to intergranular corrosion, high high-temperature strength, and superb weldability.

403 stainless steel bar

Martensitic stainless steel contains approximately 12% chromium, has high strength and hardness, moderate corrosion resistance, and can be strengthened through heat treatment.

405 stainless steel bar

Aluminum-stabilized ferritic stainless steel contains approximately 12-14% chromium.